Preparation and properties of Mo2NiB2 based cermets
-
摘要: 采用單質硼粉、鎳粉和鉬粉結合反應硼化燒結法制備了Mo2NiB2基金屬陶瓷,研究了Mo2NiB2基金屬陶瓷在燒結過程中的物相轉變和尺寸變化以及燒結溫度和保溫時間對其力學性能和顯微組織的影響.結果發現:隨著燒結溫度升高,材料物相逐漸由單質相變為二元硼化物相和三元硼化物相,并且材料的尺寸先發生細微收縮,再在硼化反應過程中逐漸增加,最后在液相燒結過程中逐漸減小;隨著燒結溫度升高,Mo2NiB2基金屬陶瓷的抗彎強度和硬度先增加后減小,在1290℃達到最大,分別為1346.5 MPa和83.7 HRA,并且硬質相顆粒逐漸粗化;保溫時間對材料性能的影響與燒結溫度一致,但在保溫30min時抗彎強度最大(1453.3 MPa),保溫60 min時硬度最大(83.7 HRA).Abstract: Mo2NiB2 based cermets were prepared using element powders of boride, nickel and molybdenum. The phase transformation and dimensional change in the sintering stage as well as the effects of sintering temperature and holding time on the mechanical properties and microstructure of Mo2NiB2 based cermets were studied. The results show that with the increasing of sintering temperature, the phase gradually transfers from elemental phase to diboride and then to ternary boride phase, the dimension of the cermets also firstly slightly decreases, then obviously increases in the boronizing sintering process, and finally significantly reduces in the subsequent liquid sintering process. The bending strength and hardness of the cermets firstly increase and then decrease when the sintering temperature rises. The cermets sintered 1290℃ for 60 min show the best mechanical properties with the bending strength of 1346.5 MPa and the hardness of 83.7 HRA. Holding time has a similar effect on the mechanical properties of the cermets. When the holding time is 30 min at 1290℃, the bending strength reaches the maximum of 1453.3 MPa.
-
Key words:
- cermets /
- microstructure /
- bending strength /
- hardness /
- phase transformation
-

計量
- 文章訪問數: 169
- HTML全文瀏覽量: 29
- PDF下載量: 8
- 被引次數: 0