Metallization of laterite lean iron ore
-
摘要: 在還原氣氛下進行了紅土貧鐵礦的還原焙燒實驗,采用正交實驗設計方法,以C/O、焙燒時間和焙燒溫度為因素,在還原氣氛下得到了最佳工藝條件為:C/O是0.8,還原焙燒溫度1350℃,時間為25min.另外發現,在更長的還原焙燒時間或焙燒溫度下,產生珠鐵分離現象.為接近實際生產條件,進行了敞開氧化氣氛實驗,由于表面氧化的原因,金屬化率僅為50%左右,通過控制球團表面氣體攪動,可減輕表面氧化現象,進而提高金屬化率,而通過氧化氣氛下的實驗結果,也證明了實際生產的可行性.Abstract: Roasting reduction of the laterite lean iron ore was tested in reduction atmosphere. The optimal pa-rameters of roasting reduction in reduction atmosphere with a metallization rate up to more than 80% were determined by orthogonal method. The roasting temperature is 1350℃, the roasting time is 25 min and C/O is 0.8. Under the condition of higher temperature or longer roasting time, a separation phenomenon of slag and iron was found. In order to accord with the practical condition, the experiment was carried out in oxidation atmosphere. Because of the oxidation layer in the surface of the pellet, the metallization rate declined to nearly 50%, and it's good for increasing the metalli-zation rate by reducing the oxidation layer. At the same time, the feasibility of roasting reduction in oxidation atmos-phere was approved by the experiment.
-
Key words:
- lean iron ore /
- roasting reduction /
- C-bearing pellet
-

計量
- 文章訪問數: 219
- HTML全文瀏覽量: 54
- PDF下載量: 4
- 被引次數: 0