Internal defects in rolled pieces during three-roll cross wedge rolling
-
摘要: 采用有限元數值模擬方法,比較分析了三輥楔橫軋與兩輥楔橫軋軋件內部缺陷的產生幾率和存在形式.根據軋件內部的應力應變狀態,闡述了三輥軋制軋件中心點缺陷產生可能性較小和斷裂呈環向裂紋的原因.分析表明,三輥楔橫軋軋制工藝在軋件心部成形質量上具有明顯的優勢.Abstract: The occurrence probability and existence form of internal defects in rolled pieces during threeroll and two-roll cross wedge rolling were compared and analyzed by finite element numerical simulation.The reason that the internal defects little occur at the center points and fissure takes an annular form during three-roll rolling was expounded based on the state of stress and strain at the center of rolled pieces. It is indicated that three-roll cross wedge rolling process has a distinct advantage in the forming quality of the center of rolled pieces.
-
Key words:
- cross wedge rolling /
- internal defects /
- finite element /
- stress /
- strain
-

計量
- 文章訪問數: 157
- HTML全文瀏覽量: 26
- PDF下載量: 7
- 被引次數: 0