Influencing Factors on Triangular Zone Cracks in a Continuously Cast Slab
-
摘要: 通過對連鑄坯硫印數據庫的分析,得到了普碳鋼連鑄板坯三角區裂紋的影響因素.結果表明,三角區裂紋隨著S含量、過熱度、拉速和鑄坯斷面寬度的增加而越來越嚴重.以此為基礎,提出了生產過程中控制三角區裂紋的原則.C含量控制為0.13%;[Mn]/[S]>25,過熱度小于25 ℃,拉速低于1.30m/min,澆鑄寬斷面鑄坯時應加強鑄坯窄邊的冷卻強度,保證良好的鑄機設備精度.Abstract: The influencing factors on triangular zone cracks were obtained by analyzing the database of sulphur printing results of continuously cast slabs. The result indicates that triangular zone cracks get worse with the increasing of sulpher content, superheat, casting speed and width of the slab. On the basis of that, the responding control principles were proposed as follows. The content of carbon should be near to the lower limit 0.13%. When the content of sulphur is between 0.015% and 0.020%, the content of manganese should be between 0.375% and 0.50% to assure the ratio of manganese to sulphur is above 25. The superheat of steel in tundish should be below 25 ℃ and the casting speed below 1.3 m/min. It is very necessary to improve the intensity of secondary cooling in the narrow side of a wider slab and ansure the precision of continuously cast machine.
-

計量
- 文章訪問數: 183
- HTML全文瀏覽量: 28
- PDF下載量: 11
- 被引次數: 0