Effect of Controlled Rolling and Cooling Process Parameters on Precipitated Pearlite of 60Si2MnA Spring Steel Wire Rods
-
摘要: 研究了60Si2MnA線材控軋控冷工藝參數對所析出的珠光體的影響.結果表明:在其他工藝參數相同的情況下,珠光體平均片層間距主要取決于吐絲到集卷過程的冷卻,這一過程冷速越快,珠光體平均片層間距越小;珠光體平均片層間距隨著吐絲溫度或終軋溫度的升高呈下降的趨勢;終軋后快冷容易出現退化珠光體,并巨其含量隨相變區冷速的加快而明顯增多;較低的終軋溫度使珠光體球團直徑明顯減小.
-
關鍵詞:
- 控軋控冷工藝參數 /
- 珠光體片層間距 /
- 珠光體球團 /
- 60Si2MnA線材
Abstract: The effect of controlled rolling and cooling process parameters on the precipitated pearlite of 60Si2MnA spring steel wire rods is carefully investigated. Experimental results show that when other process parameters are alike, the interlamellar pearlite spacing of 60Si2MnA wire rods is mainly determined by cooling rate in the process from the rod layer to the coil collecting station. The more rapid the cooling rate in this process, the thinner the interlamellar pearlite spacing. The interlamellar pearlite spacing tends to reduce with the increase of finishing temperature or rod-laying temperature. The degenerative pearlite emerges especially after cooling at a rapid rate and its content increases with the elevation of cooling rate after finish rolling. The pearlite colony becomes small obviously at a low finishing temperature. -

計量
- 文章訪問數: 198
- HTML全文瀏覽量: 58
- PDF下載量: 7
- 被引次數: 0