Cobalt-Free Maraging Alloys
-
摘要: 對含銅無鈷馬氏體時效合金系列進行了研究。固溶處理時第2相Fe2Mo完全溶解的溫度不能低于950℃。含鉬量為≤6%的合金,高溫逆轉奧氏體再結晶處理溫度為950℃;含鉬量大于6%的合金,再結晶處理的溫度,隨鉬含量增加而提高。再結晶的光學顯微組織呈長方塊狀,未再結晶的光學顯微組織呈細條束狀。540℃時效處理,主要沉淀相為Ni3Mo和Fe2Mo,前者為棒狀,后者是圓點狀。Fe-Ni15Mo6-Cu1-Ti合金,經950℃固溶和再結晶處理,540℃時效3h,常規力學性能相當于18Ni(250)的水平。Abstract: The maraging alloys series containing copper but cobalt free have been investigated. It was found that during solid solution treatment, the temperature for the second phase Fe2Mo dissolving completely could not lower than 950℃, and for the alloys containing 6% Mo or less,the recrystallization treatment temperature for high temperature reversed auste-nite was 950℃.For the alloys containing more than 6% Mo, the recrystallization treatment temperature raised with increasing Mo%.Under opi-tical microscopy the morphology after recrystallization was rectangular block shape while it was fine packet shape before recrystallization.
After solid solution and recrystallization treatments at 950℃ and aging at 540℃ for 3 h, the general mechanical properties of Fe-Nil5-Mo6-Cu4-Ti alloy were as follow:
σb=1893.3MPa, σ0.2=1784.5MPa.δ5=9.5%, (ψ)=46%,HRC=52.5.-
Key words:
- maraging alloys /
- solid solution treatment /
- recrystalliza-tion /
- reversed austenite
-

計量
- 文章訪問數: 236
- HTML全文瀏覽量: 80
- PDF下載量: 10
- 被引次數: 0