FeNiCrAl合金的顯微組織和力學性能
Microstructures and Mechanical Properties in FeNiCrAl Alloys
-
摘要: 對FeNiCrAl合金顯微組織和力學性能的研究表明:Ni/Cr0.9(摩爾比)的合金以γ相為基體,Ni/Cr(摩爾比)=0.6~0.8和0.6的合金分別以γ十α雙相和α相為基體,合金在不同溫度熱處理后,由于相的析出或溶解,顯示出不同的力學性能.Abstract: A study on microstructures and mechanical propertiesin FeMCrAl alloys was accomplished. The results showed that, when the ratio of equivalent concentrations of M and Cr, M/Cr, was higher than 0.9, the alloys formed γ-phase matrix. The alloys with M/Cr ratios of 0.6~0.8 and 0.6 formed α+γ double phases and α-phase matrixes respectively. After treating at different temperature, the phase precipitation or phase dissolution was occured. Alloys were obtained different mechanical properties.